Processing Properties | Metric | English | Comments |
---|---|---|---|
Annealing Temperature | 750 - 800 °C | 1380 - 1470 °F | Cooling: forced air or water |
Outokumpu 4713 High Temperature Ferritic Stainless Steel Does not form brittle phases but should only be exposed to moderately corrosive atmospheres due to low chromium content.Applications: Mostly used in high temperature applications with sulphurous atm.. |
|||
Annealing Temperature | 749 - 799 °C | 1380 - 1470 °F | Soft; Cooling: Furnace 20°F/hour to 1200°F/ Then air cool; < 230 HB |
Schmolz + Bickenbach Thermodur® 2344 Magnum Hot Work Die Steel Description: Thermodur® 2344 Magnum is an electro slag remelted (ESR) hot work die steel, designed to meet all die casting industry specificationCharacteristics: Excellent toughness; Excellent re.. |
|||
Annealing Temperature | 749 - 799 °C | 1380 - 1470 °F | Soft; Cooling: Furnace 20°F/hour to 1200°F/ Then air cool; < 230 HB |
Schmolz + Bickenbach Thermodur® 2365 EFS Extra Fine Structure - Hot Work Die Steel Description: Thermodur® 2365 is an Extra Fine Structure (EFS) hot work tool steel developed for good high temperature strength and tempering resistance and Supplied in the annealed conditionChara.. |
|||
Annealing Temperature | 749 - 799 °C | 1380 - 1470 °F | Soft; Cooling: Furnace 20°F/hour to 1200°F/ Then air cool; < 230 HB |
Schmolz + Bickenbach Thermodur® 2344 EFS Extra Fine Structure - Hot Work Die Steel Description: THERMODUR 2344 is a single melt Extra Fine Structure (EFS) hot work die steel; and Supplied in the annealed conditionCharacteristics: Good toughness; Good resistance to thermal shock a.. |