Processing Properties | Metric | English | Comments |
---|---|---|---|
Annealing Temperature | <= 593 °C @Time 14400 - 25200 sec |
<= 1100 °F @Time 4.00 - 7.00 hour |
Hold for time, slow cool |
Schmolz + Bickenbach 416 Stainless Steel Bar Description: Ugitech’s 416 is free machining martensitic grade. The unique production process—developed exclusively by Ugitech—results in a product that delivers superior productivity.. |