Processing Properties | Metric | English | Comments |
---|---|---|---|
Shelf Life | >= 21.0 Month | >= 21.0 Month | in closed original containers if transported and stored at temperatures between 1 and 30°C |
Struktol STRUKSILON 8023 Silicone Stabilizer for PU-Rigid Foam STRUKSILON 8023 is a universal stabilizer for polyurethane rigid foams. It is especially recommended for the use in poor in place and roof sprayfoam applications.Applications: Information provided b.. |
|||
Shelf Life | 21.0 Month | 21.0 Month | |
Dow Corning 840 RESIN Medium-hard silicone binder resin for maintenance paints, colored baking enamels, decorative finishes. Improves heat resistance and weathering of organic resins. As an additive to improve flow-out o.. |