Polymer Property : Dew Point = 23.0 °F Product List

Processing Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Processing Properties Metric English Comments
Dew Point -5.00 °C
23.0 °F
AdvanSource Biomaterials HYDROTHANE™ Hydrophilic Thermoplastic Polyurethane
AdvanSource Biomaterials Corporation manufactures and markets hydrophilic high slip, high water absorptive, polyether aliphatic polyurethanes designed for use as coatings of catheters, sutures, intr..