Processing Properties | Metric | English | Comments |
---|---|---|---|
Roll Temperature | 63.0 - 85.0 °C | 145 - 185 °F | Down Stack, Middle |
Ineos ABS Lustran® LK197 ABS, Extrusion Grade Lustran® ABS LK197 resin is a high-gloss, medium-impact extrusion grade of ABS (Acrylonitrile Butadiene Styrene). It provides a superior balance between rigidity and impact strength, as well as e.. |