Polymer Property : Roll Temperature = 302 °F Product List

Processing Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Processing Properties Metric English Comments
Roll Temperature 150 °C
302 °F
1, Extrusion
Lubrizol Estane® 54611 Polyester-Based Thermoplastic Polyurethane
Feature: Facilitates to produce high coating weight in one pass high production speed. Broad process window and transparent spherical pellets.Uses: Melt roll coated fabrics and unsupported foils.Av..
Roll Temperature 150 - 170 °C
302 - 338 °F
Hotmelt Coating Multi Roller
EMS-Griltech Griltex® D 1299A Heat Stabilized Copolyamide Hotmelt Adhesive (Technical Applications)
Description: GRILTEX adhesive products, either in pellet or powdered form, are used to coat apparel interlining substrates. Interlining substrates, coated with GRILTEX adhesive products, provides fo..
Roll Temperature 150 - 180 °C
302 - 356 °F
Hotmelt Coating Multi Roller
EMS-Griltech Griltex® D 1441E Copolyester Hotmelt Adhesive (Technical Applications)
Description: GRILTEX adhesive products, either in pellet or powdered form, are used to coat apparel interlining substrates. Interlining substrates, coated with GRILTEX adhesive products, provides fo..
Roll Temperature 150 - 190 °C
302 - 374 °F
Hotmelt Coating Multi Roller
EMS-Griltech Griltex® D 1616E Copolyester Hotmelt Adhesive (Technical Applications)
Description: GRILTEX adhesive products, either in pellet or powdered form, are used to coat apparel interlining substrates. Interlining substrates, coated with GRILTEX adhesive products, provides fo..