Processing Properties | Metric | English | Comments |
---|---|---|---|
Roll Temperature | 160 - 180 °C | 320 - 356 °F | Front |
Huntsman IROGRAN® A 85 E 4719 TPU-Polyester Introduction: IROGRAN A 85 E 4719 is a thermoplastic polyester polyurethane for melt calendering. IROGRAN is part of the HUNTSMAN technical extrusion and injection molding product range and offers a.. |
|||
Roll Temperature | 160 - 180 °C | 320 - 356 °F | Rear |
Huntsman IROGRAN® A 85 E 4719 TPU-Polyester Introduction: IROGRAN A 85 E 4719 is a thermoplastic polyester polyurethane for melt calendering. IROGRAN is part of the HUNTSMAN technical extrusion and injection molding product range and offers a.. |
|||
Roll Temperature | 160 - 180 °C | 320 - 356 °F | Front |
Huntsman IROGRAN® A 85 E 4993 FCM Polyester-Based TPU-Injection Extrusion Grade IROGRAN A 85 E 4993 FCM is a thermoplastic polyester polyurethane for melt calendaring. IROGRAN is part of the HUNTSMAN technical extrusion and injection molding product range and offers a specially.. |
|||
Roll Temperature | 160 - 180 °C | 320 - 356 °F | Rear |
Huntsman IROGRAN® A 85 E 4993 FCM Polyester-Based TPU-Injection Extrusion Grade IROGRAN A 85 E 4993 FCM is a thermoplastic polyester polyurethane for melt calendaring. IROGRAN is part of the HUNTSMAN technical extrusion and injection molding product range and offers a specially.. |
|||
Roll Temperature | 160 - 180 °C | 320 - 356 °F | Front |
Huntsman IROGRAN® A 85 E 5719 FCM TPU-Polyester Introduction: IROGRAN A 85 E 5719 FCM is a thermoplastic polyester polyurethane for melt calendering. IROGRAN is part of the HUNTSMAN technical extrusion and injection molding product range and offe.. |
|||
Roll Temperature | 160 - 180 °C | 320 - 356 °F | Rear |
Huntsman IROGRAN® A 85 E 5719 FCM TPU-Polyester Introduction: IROGRAN A 85 E 5719 FCM is a thermoplastic polyester polyurethane for melt calendering. IROGRAN is part of the HUNTSMAN technical extrusion and injection molding product range and offe.. |
|||
Roll Temperature | 150 - 180 °C | 302 - 356 °F | Hotmelt Coating Multi Roller |
EMS-Griltech Griltex® D 1441E Copolyester Hotmelt Adhesive (Technical Applications) Description: GRILTEX adhesive products, either in pellet or powdered form, are used to coat apparel interlining substrates. Interlining substrates, coated with GRILTEX adhesive products, provides fo.. |
|||
Roll Temperature | 140 - 180 °C | 284 - 356 °F | Hotmelt Coating Multi Roller |
EMS-Griltech Griltex® D 1531E Copolyester Hotmelt Adhesive (Technical Applications) Description: GRILTEX adhesive products, either in pellet or powdered form, are used to coat apparel interlining substrates. Interlining substrates, coated with GRILTEX adhesive products, provides fo.. |
|||
Roll Temperature | 160 - 180 °C | 320 - 356 °F | Hotmelt Coating Multi Roller |
EMS-Griltech Griltex® D 1533E Copolyester Hotmelt Adhesive (Technical Applications) Description: GRILTEX adhesive products, either in pellet or powdered form, are used to coat apparel interlining substrates. Interlining substrates, coated with GRILTEX adhesive products, provides fo.. |