Polymer Property : Roll Temperature = 117 °F Product List

Processing Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Processing Properties Metric English Comments
Roll Temperature 47.0 °C
117 °F
Down Stack, Middle
Ineos ABS Lustran® 256 Extrusion Blending Grade
Lustran® ABS 256 resin is a natural, medium-flow, medium-impact, low-gloss, low-gel extrusion grade of ABS (Acrylonitrile Butadiene Styrene). It is used for blending with other Lustran® ABS vi..