Processing Properties | Metric | English | Comments |
---|---|---|---|
Cure Time | 15 - 30 min | 0.25 - 0.5 hour | |
Gwent Electronic Materials R2040227D1 Hot Melt Conductive Adhesive for Diagnostic Sensors This is a one-component water based polyurethane dispersion used for bonding unsupported PVC foils. This can be used in many different diagnostic applications such as test cards, assays and support.. |