Cure Time 3.70 min
0.0617 hour
Curelastmeter
Daikin DAI-EL G-763 Fluoroelastomer Copolymer, Bisphenol Curable Grade, 66% Fluorine Content
Offers minimal compression set and excellent sealing. The copolymer type offers good compression set characteristics.Features: Excellent mold releasability for O-rings.Information provided by Daiki..