Processing Properties | Metric | English | Comments |
---|---|---|---|
Cure Time | 100 min @Temperature 25.0 °C |
1.67 hour @Temperature 77.0 °F |
Initial Set |
Chesterton ARC 5ES Rapid Repair Stick Description: ARC 5ES is specifically formulated for quick reliable repairs. Its “stick” design combines the performance of a two component system with the convenience of a single component. The AR.. |