Polymer Property : Cure Time = 0.417 hour Product List

Processing Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Processing Properties Metric English Comments
Cure Time 20.0 - 25.0 min
0.333 - 0.417 hour
working strength
Permabond TA4202 Toughened Acrylic Adhesive
PERMABOND® TA4202 is a 2-part, 1:1 toughened acrylic adhesive. It can be used to bond a wide variety of materials including metals, plastics, GRP, ceramics, wood and other substrates. It is conveni..
Cure Time 20.0 - 25.0 min
0.333 - 0.417 hour
Fixture time
ITW Devcon Metal Welderâ„¢ Methacrylate Adhesive, Grey / Beads
Information provided by ITW Devcon