Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

ITW Devcon Metal Welderâ„¢ Methacrylate Adhesive, Grey / Beads

Category Polymer , Adhesive , Thermoset , Methacrylate , Methacrylate Adhesive
Manufacturer ITW Devcon
Trade Name Metal Welder™
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF ITW Devcon Metal Welderâ„¢ Methacrylate Adhesive, Grey / Beads.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information provided by ITW Devcon
Physical Properties Metric English Comments
Viscosity 90000 cP
90000 cP
Mixed Viscosity (Thixotropic gel)
Mechanical Properties Metric English Comments
Elongation at Break 40 - 60 %
40 - 60 %
Adhesive Bond Strength 16.9 MPa
2450 psi
lap shear; ASTM D1002
Tensile Impact Strength >= 42.0 kJ/m²
>= 20.0 ft-lb/in²
Peel Strength 5.26 - 7.01 kN/m
30.0 - 40.0 pli
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 93.3 °C
200 °F
dry
Minimum Service Temperature, Air -55.0 °C
-67.0 °F
dry
Processing Properties Metric English Comments
Cure Time 4.00 - 5.00 min
0.0667 - 0.0833 hour
Working time
20.0 - 25.0 min
0.333 - 0.417 hour
Fixture time
60.0 - 120 min
1.00 - 2.00 hour
Functional cure
Descriptive Properties Value Comments
Mix ratio (Resin:Hardener) 10:1