Polymer Property : Cure Time = 0.300 hour Product List

Processing Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Processing Properties Metric English Comments
Cure Time 18.0 - 30.0 min

@Temperature 23.0 °C
0.300 - 0.500 hour

@Temperature 73.4 °F
Master Bond EP65HT-1 Fast Curing High Glass Transition Temperature Epoxy System
Master Bond Polymer System EP65HT-1 features the unusual combination of ultra-fast cures and high temperature resistance. While typical fast setting epoxies normally possess glass transition tempera..
Cure Time 18.0 min

@Temperature 25.0 °C
0.300 hour

@Temperature 77.0 °F
Trelleborg Emerson & Cuming Eccobond® 59C One-Component Silver Filled Electrically Conductive Silicone Adhesive
Emerson & Cuming 59C Eccobond® One-Component Silver Filled Electrically Conductive Silicone AdhesiveOne component, solvent containing, silver filled, electrically conductive, silicone pressure sens..
Cure Time 18.0 min

@Temperature 193 °C
0.300 hour

@Temperature 379 °F
3M Scotchkote™ 206N XTRA LG Fusion Bonded Epoxy Coating
Scotchkote Fusion Bonded Epoxy coating 206N XTRA LG is one-part, heat curable, thermosetting, powdered epoxy coating with extended gel for coating the interior of line pipe and fittings, valves, and..