3M Scotchkote™ 206N XTRA LG Fusion Bonded Epoxy Coating

Category Polymer , Thermoset , Epoxy
Manufacturer 3M
Trade Name Scotchkote™
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF 3M Scotchkote™ 206N XTRA LG Fusion Bonded Epoxy Coating.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Scotchkote Fusion Bonded Epoxy coating 206N XTRA LG is one-part, heat curable, thermosetting, powdered epoxy coating with extended gel for coating the interior of line pipe and fittings, valves, and couplers. Scotchkote coating 206N XTRA LG is NSF/ANSI 61 certified for potable water applications and is also resistant to corrosive soils, hydrocarbons, harsh chemicals and sea water. Scotchkote coating 206N XTRA LG meets the requirements of ASSA Standard C213 and C550.Information provided by 3M
Physical Properties Metric English Comments
Density 1.47 g/cc
0.0531 lb/in³
Water Absorption 1.46 %
1.46 %
ASTM D570-95
Water Vapor Transmission 4.05 g/m²/day
0.261 g/100 in²/day
ASTM D1653
Mechanical Properties Metric English Comments
Impact Test 18.1 J
13.3 ft-lb
0.32 cm x 7.6 cm x 7.6 cm, 1.6 cm diameter tup; ASTM G14
Abrasion 0.11
0.11
[g]; ASTM D4060
Electrical Properties Metric English Comments
Dielectric Strength 52.95 kV/mm
1345 kV/in
Processing Properties Metric English Comments
Cure Time 18.0 min

@Temperature 193 °C
0.300 hour

@Temperature 379 °F
Gel Time 0.666666 - 1.00 min

@Temperature 232 °C
0.666666 - 1.00 min

@Temperature 450 °F
1.50 - Error in fixSigDigits: @digits must be between 1 and 12. @digits is: 15 min

@Temperature 193 °C
1.50 - Error in fixSigDigits: @digits must be between 1 and 12. @digits is: 15 min

@Temperature 379 °F
Shelf Life 12.0 Month
12.0 Month
Descriptive Properties Value Comments
Appearance Light Gray, Mid Gray, Dark Gray, Stone, Red, Mid Green
Users viewing this material also viewed the following: