Polymer Property : Cure Time = 0.283 hour Product List

Processing Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Processing Properties Metric English Comments
Cure Time 9.00 - 17.0 min
0.150 - 0.283 hour
t`90; ASTM D2084
ExxonMobil Exxon™ 1068
Exxon Chloromobutyl is a chlorinated copolymer of isobutylene and isoprene.Information provided by ExxonMobil Chemical
Cure Time 9.00 - 17.0 min
0.150 - 0.283 hour
t`90; ASTM D2084
ExxonMobil Exxon™ 1066
Exxon Chloromobutyl is a chlorinated copolymer of isobutylene and isoprene.Information provided by ExxonMobil Chemical