Processing Properties | Metric | English | Comments |
---|---|---|---|
Cure Time | 9.00 min @Temperature 68.3 °C |
0.150 hour @Temperature 155 °F |
|
TSE Industries Millathane® E34 Millable Polyether Polyurethane Rubber with 3.0 PHR MBT MILLATHANE E34 is a high performance polyether polyurethane rubber for applications requiring: high abrasion resistance, low temperature flexibility, ozone resistance, oil and fuel resistance, outst.. |
|||
Cure Time | 9.00 min @Temperature 177 °C |
0.150 hour @Temperature 350 °F |
|
TSE Industries Millathane® HT High Temperature-Resistant Millable Polyester Polyurethane, 350ºF Cure Temperature MILLATHANE HT is a polyester millable polyurethane which has the ability to withstand elevated temperatures. Polyurethanes have been known for their excellent resistance to abrasion, impact, tear st.. |
|||
Cure Time | 9.00 - 10.0 min | 0.150 - 0.167 hour | Fixture time |
ITW Devcon Flex Bondâ„¢ Methacrylate Adhesive Pipe Sealant, Purple Information provided by ITW Devcon |
|||
Cure Time | 9.00 - 12.0 min | 0.150 - 0.200 hour | Working time |
ITW Devcon Flex Welderâ„¢ Methacrylate Adhesive, Off-White Information provided by ITW Devcon |
|||
Cure Time | 9.00 min @Temperature 177 °C |
0.150 hour @Temperature 350 °F |
|
TSE Industries Millathane® HT High Temperature-Resistant Millable Polyester Polyurethane, 350ºF Cure Temperature MILLATHANE HT is a polyester millable polyurethane which has the ability to withstand elevated temperatures. Polyurethanes have been known for their excellent resistance to abrasion, impact, tear st.. |
|||
Cure Time | 9.00 - 60.0 min | 0.150 - 1.00 hour | |
Master Bond Supreme 10AOHT-LO High Shear and Peel Strength Epoxy Description: Master Bond Supreme 10AOHT-LO has a combination of properties consisting of excellent thermal conductivity, superior electrical insulation, great adhesion to a wide variety of substrate.. |
|||
Cure Time | 9.00 min @Temperature 68.3 °C |
0.150 hour @Temperature 155 °F |
|
TSE Industries Millathane® E34 Millable Polyether Polyurethane Rubber with 3.0 PHR MBT MILLATHANE E34 is a high performance polyether polyurethane rubber for applications requiring: high abrasion resistance, low temperature flexibility, ozone resistance, oil and fuel resistance, outst.. |
|||
Cure Time | 9.00 min | 0.150 hour | Cure Time to 90% Shore D |
Chesterton ARC 5ES Rapid Repair Stick Description: ARC 5ES is specifically formulated for quick reliable repairs. Its “stick” design combines the performance of a two component system with the convenience of a single component. The AR.. |
|||
Cure Time | 9.00 - 17.0 min | 0.150 - 0.283 hour | t`90; ASTM D2084 |
ExxonMobil Exxon™ 1068 Exxon Chloromobutyl is a chlorinated copolymer of isobutylene and isoprene.Information provided by ExxonMobil Chemical |
|||
Cure Time | 9.00 min | 0.150 hour | t`90, Target; ASTM D2084 |
ExxonMobil Exxon™ 2235 Regular Cure Rate Grade Exxon Bromobutyl is a brominated copolymer of isobutylene and isoprene. The product form is white to light amber bales.Information provided by ExxonMobil Chemical |
|||
Cure Time | 9.00 min | 0.150 hour | t`90, Target; ASTM D2084 |
ExxonMobil Exxon™ 2244 Fast Cure Rate Grade Exxon Bromobutyl is a brominated copolymer of isobutylene and isoprene. The product form is offwhite to amber bales.Information provided by ExxonMobil Chemical |
|||
Cure Time | 9.00 min @Temperature 100 °C |
0.150 hour @Temperature 212 °F |
|
Dow Corning 3-4170 DIELECTRIC GEL KIT Two-part, clear, heat cure, long working time.Information provided by Dow Corning |
|||
Cure Time | 9.00 - 10.0 min | 0.150 - 0.167 hour | Tack-Free |
3M Scotch-Weld™ DP100 Plus Clear Epoxy Adhesive 3M™ Scotch-Weld™ Epoxy Adhesive DP100 Plus Clear is a fast setting, two-part, 1:1 mix ratio mercaptan-cured epoxy adhesive. It is a unique among fast setting mercaptan cure epoxies in that it comb.. |
|||
Cure Time | 9.00 - 17.0 min | 0.150 - 0.283 hour | t`90; ASTM D2084 |
ExxonMobil Exxon™ 1066 Exxon Chloromobutyl is a chlorinated copolymer of isobutylene and isoprene.Information provided by ExxonMobil Chemical |