Processing Properties | Metric | English | Comments |
---|---|---|---|
Cure Time | 0.183 min | 0.00306 hour | fixture time, (low power 4mW lamp) |
Permabond UV610 UV-curable Adhesive PERMABOND UV610 is a single part, fast setting, UV curable adhesive designed specifically for bonding glass and metal. Its high strength makes it suitable for a wide range of applications including .. |