Processing Properties Metric English Comments
Cure Time 0.0667 - 0.417 min
0.00111 - 0.00695 hour
Time to Handling Strength
3M Scotch-Weld™ PR600 Plastic and Rubber Instant Adhesive
3M™ Scotch-Weld™ Plastic and Rubber Instant Adhesive is designed to give exceptional performance on difficult-to-bond plastic and rubber substrates. This adhesive may be bonded to like substrates ..
Cure Time 0.0667 - 0.417 min
0.00111 - 0.00695 hour
Time to Handling Strength
3M Scotch-Weld™ PR600B Plastic and Rubber Instant Adhesive
3M™ Scotch-Weld™ Plastic and Rubber Instant Adhesive is designed to give exceptional performance on difficult-to-bond plastic and rubber substrates. This adhesive may be bonded to like substrates ..