3M Scotch-Weld™ PR600 Plastic and Rubber Instant Adhesive

Category Polymer , Adhesive
Manufacturer 3M
Trade Name Scotch-Weld™
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF 3M Scotch-Weld™ PR600 Plastic and Rubber Instant Adhesive.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
3M™ Scotch-Weld™ Plastic and Rubber Instant Adhesive is designed to give exceptional performance on difficult-to-bond plastic and rubber substrates. This adhesive may be bonded to like substrates or in combination with metal or composite substrates. Superior performance is achieved on materials such as heavily plasticized PVC, EPDM, ABS, Nylon, Santoprene® and Viton®. PR600 is a medium viscosity cyanoacrylate with some gap-filling capability. It will bond many common substrates including plastics and rubbers. It has been tested and passed the requirements of Commercial Item Description A-A-3097, Type II Class 3 (formerly MIL-A-46050C).Information provided by 3M
Physical Properties Metric English Comments
Density 1.07 g/cc
0.0387 lb/in³
Brookfield Viscosity 510 - 660 cP
510 - 660 cP
LVF, sp 3 @ 30 rpm
Mechanical Properties Metric English Comments
Shear Strength 20.0 MPa
2900 psi
cured, grit-blasted steel; ASTM D1002
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 82.0 °C
180 °F
Minimum Service Temperature, Air -54.0 °C
-65.2 °F
Processing Properties Metric English Comments
Cure Time 0.0667 - 0.417 min
0.00111 - 0.00695 hour
Time to Handling Strength
1440 min
24.0 hour
Full Cure
Descriptive Properties Value Comments
Appearance Clear Liquid