Processing Properties Metric English Comments
Back Pressure 6.00 - 18.0 MPa
870 - 2610 psi
PTS PBT-20GFR 20% Glass Filled
PBT, injection molding grade, 20% glass fiber reinforced, flame retardant, exceptional flowability and processability, colorable.Information provided by PTS LLC.
Back Pressure 6.00 - 18.0 MPa
870 - 2610 psi
Beijing Ranger Chem PBT 403 M-G20 Heat Resistant and Environmental Protection Flame Retarding FR PBT
Modified PBT Characteristics: Unreinforced grades have abundant strength and flexibility, and have strong characteristics against brittleness. UL-certified slow-burning (94HB) and self-extinguishin..
Back Pressure 6.00 - 18.0 MPa
870 - 2610 psi
Beijing Ranger Chem PBT 403 M-G20 HF Halogen Free Flame Retarding FR PBT
Modified PBT Characteristics: Unreinforced grades have abundant strength and flexibility, and have strong characteristics against brittleness. UL-certified slow-burning (94HB) and self-extinguishin..
Back Pressure 6.00 - 18.0 MPa
870 - 2610 psi
Beijing Ranger Chem PBT-201-G20 272 Flame Retarding FR PBT
Modified PBT Characteristics: Unreinforced grades have abundant strength and flexibility, and have strong characteristics against brittleness. UL-certified slow-burning (94HB) and self-extinguishin..
Back Pressure 6.00 - 18.0 MPa
870 - 2610 psi
Beijing Ranger Chem PBT-MFC-G20 FR PBT
Modified PBT Characteristics: Unreinforced grades have abundant strength and flexibility, and have strong characteristics against brittleness. UL-certified slow-burning (94HB) and self-extinguishin..
Back Pressure 6.00 - 18.0 MPa
870 - 2610 psi
BLUESTAR PBT 403M-G30 30% Glass Filled
PBT, injection molding grade, 30% glass fiber reinforced, flame retardant, exceptional flowability and processability, colorableInformation provided by Polymer Technology and Services, LLC (PTS).
Back Pressure 6.00 - 18.0 MPa
870 - 2610 psi
Beijing Chemical Industry KAIFA® 301-G20 PBT Resin
20% glass fiber reinforced, flame retardantInformation provided by Beijing Chemical Industry Research Institute (Group)
Back Pressure 6.00 - 18.0 MPa
870 - 2610 psi
Beijing Chemical Industry KAIFA® 301-G30 PBT Resin
30% glass fiber reinforced, flame retardantInformation provided by Beijing Chemical Industry Research Institute (Group)
Back Pressure 6.00 - 18.0 MPa
870 - 2610 psi
Beijing Ranger Chem PBT-201-G20 202 Environmental Protection Flame Retarding FR PBT
Modified PBT Characteristics: Unreinforced grades have abundant strength and flexibility, and have strong characteristics against brittleness. UL-certified slow-burning (94HB) and self-extinguishin..
Back Pressure 6.00 - 18.0 MPa
870 - 2610 psi
Beijing Ranger Chem PBT-201-G20 Flame Retarding FR PBT
Modified PBT Characteristics: Unreinforced grades have abundant strength and flexibility, and have strong characteristics against brittleness. UL-certified slow-burning (94HB) and self-extinguishin..
Back Pressure 6.00 - 18.0 MPa
870 - 2610 psi
BLUESTAR PBT 403M-G20 20% Glass Filled
PBT, injection molding grade, 20% glass fiber reinforced, flame retardant, exceptional flowability and processability, colorable.Information provided by Polymer Technology and Services, LLC (PTS).