Processing Properties | Metric | English | Comments |
---|---|---|---|
Back Pressure | 6.00 - 18.0 MPa | 870 - 2610 psi | |
PTS PBT-20GFR 20% Glass Filled PBT, injection molding grade, 20% glass fiber reinforced, flame retardant, exceptional flowability and processability, colorable.Information provided by PTS LLC. |
|||
Back Pressure | 8.00 - 18.0 MPa | 1160 - 2610 psi | |
Zhejiang Juner 201-G20 20% Glass Fibre Reinforced Applications: Electrons and Electricity: TV Components, Plugs of Computers, Exhaust Fans of Computers, Plugs, Sockets, Shells of Electronics, Framework of Level Output Transformers, Pipe Pedestals, .. |
|||
Back Pressure | 8.00 - 18.0 MPa | 1160 - 2610 psi | |
Zhejiang Juner 201-G30 30% Glass Fibre Reinforced Applications: Electrons and Electricity: TV Components, Plugs of Computers, Exhaust Fans of Computers, Plugs, Sockets, Shells of Electronics, Framework of Level Output Transformers, Pipe Pedestals, .. |
|||
Back Pressure | 8.00 - 18.0 MPa | 1160 - 2610 psi | |
Beijing Chemical Industry KAIFA® 201-G15R PBT Resin 20% glass fiber reinforced, good flow and toughnessInformation provided by Beijing Chemical Industry Research Institute (Group) |
|||
Back Pressure | 8.00 - 18.0 MPa | 1160 - 2610 psi | |
Beijing Chemical Industry KAIFA® 201-G20R PBT Resin 15% glass fiber reinforced, good flow and toughnessInformation provided by Beijing Chemical Industry Research Institute (Group) |
|||
Back Pressure | 8.00 - 18.0 MPa | 1160 - 2610 psi | |
Beijing Chemical Industry KAIFA® 201-G30R PBT Resin 30% glass fiber reinforced, good flow and toughnessInformation provided by Beijing Chemical Industry Research Institute (Group) |
|||
Back Pressure | 8.00 - 18.0 MPa | 1160 - 2610 psi | |
Beijing Chemical Industry KAIFA® 2030 PET Resin High mechanical strength, Creep resistant, Low frictionInformation provided by Beijing Chemical Industry Research Institute (Group) |
|||
Back Pressure | 8.00 - 18.0 MPa | 1160 - 2610 psi | |
Beijing Chemical Industry KAIFA® 301-G0F PBT Resin Flame retardant, good flow, low bleedingInformation provided by Beijing Chemical Industry Research Institute (Group) |
|||
Back Pressure | 8.00 - 18.0 MPa | 1160 - 2610 psi | |
Beijing Chemical Industry KAIFA® 301-G10F PBT Resin 10% glass fiber reinforced, flame retardant, good flow, low bleedingInformation provided by Beijing Chemical Industry Research Institute (Group) |
|||
Back Pressure | 6.00 - 18.0 MPa | 870 - 2610 psi | |
Beijing Ranger Chem PBT 403 M-G20 Heat Resistant and Environmental Protection Flame Retarding FR PBT Modified PBT Characteristics: Unreinforced grades have abundant strength and flexibility, and have strong characteristics against brittleness. UL-certified slow-burning (94HB) and self-extinguishin.. |
|||
Back Pressure | 6.00 - 18.0 MPa | 870 - 2610 psi | |
Beijing Ranger Chem PBT 403 M-G20 HF Halogen Free Flame Retarding FR PBT Modified PBT Characteristics: Unreinforced grades have abundant strength and flexibility, and have strong characteristics against brittleness. UL-certified slow-burning (94HB) and self-extinguishin.. |
|||
Back Pressure | 8.00 - 18.0 MPa | 1160 - 2610 psi | |
Beijing Ranger Chem PBT 403 M-G30 Heat Resistant and Environmental Protection Flame Retarding FR PBT Modified PBT Characteristics: Unreinforced grades have abundant strength and flexibility, and have strong characteristics against brittleness. UL-certified slow-burning (94HB) and self-extinguishin.. |
|||
Back Pressure | 6.00 - 18.0 MPa | 870 - 2610 psi | |
Beijing Ranger Chem PBT-201-G20 272 Flame Retarding FR PBT Modified PBT Characteristics: Unreinforced grades have abundant strength and flexibility, and have strong characteristics against brittleness. UL-certified slow-burning (94HB) and self-extinguishin.. |
|||
Back Pressure | 6.00 - 18.0 MPa | 870 - 2610 psi | |
Beijing Ranger Chem PBT-MFC-G20 FR PBT Modified PBT Characteristics: Unreinforced grades have abundant strength and flexibility, and have strong characteristics against brittleness. UL-certified slow-burning (94HB) and self-extinguishin.. |
|||
Back Pressure | 6.00 - 18.0 MPa | 870 - 2610 psi | |
BLUESTAR PBT 403M-G30 30% Glass Filled PBT, injection molding grade, 30% glass fiber reinforced, flame retardant, exceptional flowability and processability, colorableInformation provided by Polymer Technology and Services, LLC (PTS). |
|||
Back Pressure | 8.00 - 18.0 MPa | 1160 - 2610 psi | |
Beijing Chemical Industry KAIFA® 201-G0R PBT Resin Good flow and toughnessInformation provided by Beijing Chemical Industry Research Institute (Group) |
|||
Back Pressure | 8.00 - 18.0 MPa | 1160 - 2610 psi | |
Beijing Chemical Industry KAIFA® 201-G30 PBT Resin 30% glass fiber reinforcedInformation provided by Beijing Chemical Industry Research Institute (Group) |
|||
Back Pressure | 8.00 - 18.0 MPa | 1160 - 2610 psi | |
Beijing Chemical Industry KAIFA® 301-G15F PBT Resin 15% glass fiber reinforced, flame retardant, good flow, low bleedingInformation provided by Beijing Chemical Industry Research Institute (Group) |
|||
Back Pressure | 8.00 - 18.0 MPa | 1160 - 2610 psi | |
Beijing Chemical Industry KAIFA® 301-G15RF PBT Resin 15% glass fiber reinforced, flame retardant, good toughness, low bleedingInformation provided by Beijing Chemical Industry Research Institute (Group) |
|||
Back Pressure | 6.00 - 18.0 MPa | 870 - 2610 psi | |
Beijing Chemical Industry KAIFA® 301-G20 PBT Resin 20% glass fiber reinforced, flame retardantInformation provided by Beijing Chemical Industry Research Institute (Group) |
|||
Back Pressure | 8.00 - 18.0 MPa | 1160 - 2610 psi | |
Beijing Chemical Industry KAIFA® 301-G20F PBT Resin 20% glass fiber reinforced, flame retardant, good flow, low bleedingInformation provided by Beijing Chemical Industry Research Institute (Group) |
|||
Back Pressure | 6.00 - 18.0 MPa | 870 - 2610 psi | |
Beijing Chemical Industry KAIFA® 301-G30 PBT Resin 30% glass fiber reinforced, flame retardantInformation provided by Beijing Chemical Industry Research Institute (Group) |
|||
Back Pressure | 8.00 - 18.0 MPa | 1160 - 2610 psi | |
Beijing Chemical Industry KAIFA® 301-G30F PBT Resin 30% glass fiber reinforced, flame retardant, good flow, low bleedingInformation provided by Beijing Chemical Industry Research Institute (Group) |
|||
Back Pressure | 8.00 - 18.0 MPa | 1160 - 2610 psi | |
Beijing Chemical Industry KAIFA® 3030F PET Resin High mechanical strength, Creep resistant, Low friction, High crystallizationInformation provided by Beijing Chemical Industry Research Institute (Group) |
|||
Back Pressure | 6.00 - 18.0 MPa | 870 - 2610 psi | |
Beijing Ranger Chem PBT-201-G20 202 Environmental Protection Flame Retarding FR PBT Modified PBT Characteristics: Unreinforced grades have abundant strength and flexibility, and have strong characteristics against brittleness. UL-certified slow-burning (94HB) and self-extinguishin.. |
|||
Back Pressure | 6.00 - 18.0 MPa | 870 - 2610 psi | |
Beijing Ranger Chem PBT-201-G20 Flame Retarding FR PBT Modified PBT Characteristics: Unreinforced grades have abundant strength and flexibility, and have strong characteristics against brittleness. UL-certified slow-burning (94HB) and self-extinguishin.. |
|||
Back Pressure | 8.00 - 18.0 MPa | 1160 - 2610 psi | |
Beijing Ranger Chem PBT-201-G30 272 Flame Retarding FR PBT Modified PBT Characteristics: Unreinforced grades have abundant strength and flexibility, and have strong characteristics against brittleness. UL-certified slow-burning (94HB) and self-extinguishin.. |
|||
Back Pressure | 8.00 - 18.0 MPa | 1160 - 2610 psi | |
Beijing Ranger Chem PBT-201-G30 Flame Retarding FR PBT Modified PBT Characteristics: Unreinforced grades have abundant strength and flexibility, and have strong characteristics against brittleness. UL-certified slow-burning (94HB) and self-extinguishin.. |
|||
Back Pressure | 8.00 - 18.0 MPa | 1160 - 2610 psi | |
Beijing Ranger Chem PBT-MFC-G30 FR PBT Modified PBT Characteristics: Unreinforced grades have abundant strength and flexibility, and have strong characteristics against brittleness. UL-certified slow-burning (94HB) and self-extinguishin.. |
|||
Back Pressure | 6.00 - 18.0 MPa | 870 - 2610 psi | |
BLUESTAR PBT 403M-G20 20% Glass Filled PBT, injection molding grade, 20% glass fiber reinforced, flame retardant, exceptional flowability and processability, colorable.Information provided by Polymer Technology and Services, LLC (PTS). |