Polymer Property : Back Pressure = 500 psi Product List

Processing Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Processing Properties Metric English Comments
Back Pressure 1.72 - 3.45 MPa
250 - 500 psi
PTS PCA-3013 High Flow PC/PBT Alloy
Information provided by Polymer Technology and Services, LLC (PTS).
Back Pressure 0.000 - 3.45 MPa
0.000 - 500 psi
PTS PCA-3015 Low Temperature Impact PC/PBT Alloy
Information provided by Polymer Technology and Services, LLC (PTS).
Back Pressure 0.345 - 3.45 MPa
50.0 - 500 psi
Styron MAGNUMâ„¢ 347 HP Acrylonitrile Butadiene Styrene (ABS) Resin
Overview: MAGNUMâ„¢ ABS resins are thermoplastic materials which provide an excellent balance of processability, impact resistance and heat resistance as imparted by the various polymer compositi..
Back Pressure 1.03 - 3.45 MPa
149 - 500 psi
Styron Magnum™ 1150 EM Acrylonitrile Butadiene Styrene (ABS)
Overview: MAGNUM™ ABS resins are thermoplastic materials which provide an excellent balance to processability, impact resistance and heat resistance as imparted by the various polymer compositions...