Polymer Property : Dry Time = 1 hour Product List

Processing Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Processing Properties Metric English Comments
Dry Time 0.5 - 1 hour
0.5 - 1 hour
Touch
Aremco Aremco-Seal™ FO-380 High Temperature Specialty Coatings Silicone, Ceramic Filled  (discontinued **)
Hi-temp, waterborne silicone adhesive and sealant used to pot fiber optic strands into stainless steel ferrules. Typically used in applications to 716 °F (380 °C). Low viscosity, easy to use, offe..
Dry Time 0.5 - 1 hour
0.5 - 1 hour
Lord Adhesives Chemlok® 485/Curative 44 Adhesive
LORD Chemlok® 485/Curative 44 adhesive is a two component adhesive system used for insert mold bonding of PVC and Alcryn® to substrates such as metal, rubber and other thermoplastic elastomers..
Dry Time 0.5 - 1 hour
0.5 - 1 hour
Recoat
Aremco Aremco-Seal™ 613 High Temperature Specialty Coatings Glass
Dry Time 0.5 - 1 hour
0.5 - 1 hour
Recoat
Aremco Aremco-Seal™ 617 High Temperature Specialty Coatings Glass
Glass coating for producing hermetic seals in porous ceramics and refractories to 1450 ºF. Used for sealing high vacuum components, resistance temperature devices, and other electrical sensors.