Processing Properties | Metric | English | Comments |
---|---|---|---|
Dry Time | 2.00 hour | 2.00 hour | |
PolyOne OnFlex™ S KE 60A-3S1725 Thermoplastic Elastomer (TPE) OnFlex™-S KE thermoplastic elastomer compounds are based on hydrogenated styrenic block copolymers. This range of compounds are specially compatabilized to provide excellent adhesion to a variety p.. |
|||
Dry Time | 2.00 hour | 2.00 hour | |
PolyOne OnForce™ LFT PP-60LGF/001 Natural Polypropylene Homopolymer (PP Homopolymer) PolyOne's Long Fiber Thermoplastic (LFT) compounds are formulated for demanding applications which require high stiffness and good impact such as metal replacement or other structural applications. .. |
|||
Dry Time | 2.00 hour | 2.00 hour | |
PolyOne Edgetek® XT XT-100-BW00 Natural Polycarbonate + PBT (PC+PBT) EDGETEK™ XT High Performance Polymers are polycarbonate and polyester alloys that combine strength, durability and chemical resistance. The Edgetek XT product family includes a complete line of gen.. |
|||
Dry Time | 2.00 - 4.00 hour | 2.00 - 4.00 hour | |
DuPont Performance Polymers Crastin® S600F10 BK851 PBT
(Unverified Data**) Crastin® S600F10 BK851 is an unreinforced, lubricated, medium high viscosity, black polybutylene terephthalate resin for injection molding.Information provided by DuPont Performance Polymers |
|||
Dry Time | 2.00 - 4.00 hour | 2.00 - 4.00 hour | |
DuPont Performance Polymers Crastin® SK609 BK851 PBT
(Unverified Data**) Crastin® SK609 BK851 is a 50% glass fiber reinforced, lubricated, black polybutylene terephthalate resin for injection molding.Information provided by DuPont Performance Polymers |
|||
Dry Time | 2.00 - 3.00 hour | 2.00 - 3.00 hour | Dehumidified Dryer; Injection Molding |
DuPont Performance Polymers Hytrel® 7246HS BK320 TPC-ET
(Unverified Data**) Hytrel® 7246HS BK320 is a high modulus, heat stabilized, black grade with nominal hardness of 72D.Information provided by DuPont |
|||
Dry Time | 2.00 - 3.00 hour | 2.00 - 3.00 hour | Extrusion |
DuPont Performance Polymers Hytrel® HTR8730 BK320 TPC-ET
(Unverified Data**) Hytrel® HTR8730 BK320 is a high viscosity thermoplastic polyester elastomer designed for blow molding. It has excellent mechanical properties at elevated temperatures and very good resistance to mo.. |
|||
Dry Time | 2.00 - 4.00 hour | 2.00 - 4.00 hour | Injection Molding |
DuPont Performance Polymers Delrin® 327UVE RD402 Acetal Homopolymer
(Unverified Data**) Delrin® 327UVE RD402 (formerly DE20554) is a medium-high viscosity acetal homopolymer with UV stabilizers having extremely low VOC emissions, developed for automotive interior applications.Informat.. |
|||
Dry Time | 2.00 - 3.00 hour | 2.00 - 3.00 hour | Injection Molding |
LG Chemical LUCEL FW700N Modified POM, Friction Resistance, Abrasion Resistance Feature: Injection Molding, Modified POM, Friction Resistance, Abrasion ResistanceApplication: Gears, Printer Roller Pumps, Gear Worm WheelsCAS No. 66455-31-0Information provided by LG Chemical |
|||
Dry Time | 2.00 - 6.00 hour | 2.00 - 6.00 hour | |
Gromax BTE30-DN00N1 Nylon 6 (Conditioned) Information provided by Gromax Enterprises Corp. |
|||
Dry Time | 2.00 - 6.00 hour | 2.00 - 6.00 hour | |
Gromax BTE35-DN00N1 Nylon 6 (Dry) Information provided by Gromax Enterprises Corp. |
|||
Dry Time | 2.00 - 6.00 hour | 2.00 - 6.00 hour | |
Gromax BTE70-FN001N1 Nylon 6 (Dry) Information provided by Gromax Enterprises Corp. |
|||
Dry Time | 2.00 - 6.00 hour @Temperature 80.0 °C |
2.00 - 6.00 hour @Temperature 176 °F |
|
Lanxess Durethan® BKV 135 DUS008 000000 Nylon 6, 35% Glass Fiber PA 6, 35% glass fibers, injection molding, impact modifiedInformation provided by LANXESS. |
|||
Dry Time | 2.00 - 6.00 hour @Temperature 80.0 °C |
2.00 - 6.00 hour @Temperature 176 °F |
|
Lanxess Durethan® BKV 230 DUS008 000000 Nylon 6, 30% Glass Fiber PA 6, 30% glass fiber, injection molding, impact modified, heat-ageing stabilizedInformation provided by LANXESS. |
|||
Dry Time | 2.00 - 6.00 hour | 2.00 - 6.00 hour | |
Gromax BTE65-DN001N1 Nylon 6 (Conditioned) Information provided by Gromax Enterprises Corp. |
|||
Dry Time | 2.00 - 6.00 hour @Temperature 80.0 °C |
2.00 - 6.00 hour @Temperature 176 °F |
|
Lanxess Durethan® BKV 115 DUS008 000000 Nylon 6, 15% Glass Fiber PA 6, 15% glass fibers, injection molding, impact modified, heat-ageing stabilizedInformation provided by LANXESS. |
|||
Dry Time | 2.00 - 4.00 hour | 2.00 - 4.00 hour | |
Lubrizol ESTALOC® 59300 Polyester-Type, Reinforced Engineering Thermoplastic Polyurethane Features: Fast Cycling, Dimensional Stability, Durability, Aesthetics, Low Temperature ImpactUses: Injection MoldingAvailability: Americas, Europe, Middle East, Africa, India and AsiaInformation pro.. |
|||
Dry Time | 2.00 - 4.00 hour | 2.00 - 4.00 hour | |
Eurotec® Tecodur® PB70 GR10 NL100 PBT, 10% glass fiber reinforced, natural Information provided by Eurotec® |
|||
Dry Time | 2.00 - 4.00 hour | 2.00 - 4.00 hour | |
Eurotec® Tecomid® NA30 GR50 BK002 XA40 PA6.6, 50% glass fiber reinforced, flame retardant, heat stabilized, natural Information provided by Eurotec® |
|||
Dry Time | 2.00 - 4.00 hour | 2.00 - 4.00 hour | |
Eurotec® Tecomid® NA40 GR14 NL MC PA6.6, 14% glass fiber reinforced, impact modified, heat stabilized, natural Information provided by Eurotec® |
|||
Dry Time | 2.00 - 4.00 hour | 2.00 - 4.00 hour | |
Eurotec® Tecomid® NA40 GR30 NL RT PA6.6, 30% glass fiber reinforced, PTFE modified, natural Information provided by Eurotec® |
|||
Dry Time | 2.00 - 4.00 hour | 2.00 - 4.00 hour | |
Eurotec® Tecomid® NB40 GR30 NL IM PA6, 30% glass fiber reinforced, impact modified, natural Information provided by Eurotec® |
|||
Dry Time | 2.00 - 4.00 hour | 2.00 - 4.00 hour | |
Eurotec® Tecomid® NA40 GR13 NL100 MB PA6.6, 13% glass fiber reinforced, impact modified, heat stabilized, natural Information provided by Eurotec® |
|||
Dry Time | 2.00 - 4.00 hour | 2.00 - 4.00 hour | |
Eurotec® Tecomid® NB40 GR15 NL HS PA6, 15% glass fiber reinforced, heat stabilized, natural Information provided by Eurotec® |
|||
Dry Time | 2.00 - 4.00 hour | 2.00 - 4.00 hour | Injection Molding |
DuPont Performance Polymers Delrin® 900P BK602 Acetal Homopolymer
(Unverified Data**) Delrin® 900P BK602 is a low viscosity black acetal homopolymer resin for multicavity and thin wall molding. It offers an improved processing thermal stability.Information provided by DuPont Perform.. |
|||
Dry Time | 2.00 - 4.00 hour | 2.00 - 4.00 hour | |
Eurotec® Tecomid® NB40 MR25 NL IL PA6, 25% mineral reinforced, impact modified, natural Information provided by Eurotec® |
|||
Dry Time | 2.00 - 4.00 hour | 2.00 - 4.00 hour | |
Eurotec® Tecomid® NB40 NL E PA6, unfilled, natural Information provided by Eurotec® |