Polymer Property : Drying Temperature = 260 °F Product List

Processing Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Processing Properties Metric English Comments
Drying Temperature 118 - 127 °C
245 - 260 °F
Average value: 123 °C Grade Count:9
Overview of materials for Polycarbonate, Foam Grade, Glass Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, Foam Grade, Glass Filled". Each property range of values reported is minimum and maximum ..
Drying Temperature 120 - 127 °C
248 - 260 °F
Average value: 125 °C Grade Count:36
Overview of materials for Polytrimethylene Terephthalate (PTT)
This property data is a summary of similar materials in the MatWeb database for the category "Polytrimethylene Terephthalate (PTT)". Each property range of values reported is minimum and maximum val..