Processing Properties | Metric | English | Comments |
---|---|---|---|
Drying Temperature | 118 - 127 °C | 245 - 260 °F | Average value: 123 °C Grade Count:9 |
Overview of materials for Polycarbonate, Foam Grade, Glass Filled This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, Foam Grade, Glass Filled". Each property range of values reported is minimum and maximum .. |
|||
Drying Temperature | 120 - 127 °C | 248 - 260 °F | Average value: 125 °C Grade Count:36 |
Overview of materials for Polytrimethylene Terephthalate (PTT) This property data is a summary of similar materials in the MatWeb database for the category "Polytrimethylene Terephthalate (PTT)". Each property range of values reported is minimum and maximum val.. |