Polymer Property : Mold Temperature = 71.6 °F Product List

Processing Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Processing Properties Metric English Comments
Mold Temperature 10.0 - 22.0 °C
50.0 - 71.6 °F
Lubrizol Estane® 58144 Thermoplastic Polyurethane
Type: Estane® 58144 is a 65D Polyether-type thermoplastic polyurethane (TPU) compound.Features: FDA (contact Lubrizol for details). Pre-drying: 2 hours at 104C (220F) in Dehumidifying Hopper Dryer..