Processing Properties | Metric | English | Comments |
---|---|---|---|
Mold Temperature | 140 - 230 °C | 284 - 446 °F | short vulcanization time required (a few seconds) |
Momentive Performance Materials Siloprenâ„¢ Electro 242-1 Electrically Insulating Liquid Silicone Rubber This LSR elastomer is an electrically insulating, two-component, platinum (addition/heat) curable, and pumpable silicone elastomer that can be molded and cured with very fast cycle times, at elevate.. |
|||
Mold Temperature | 140 - 230 °C | 284 - 446 °F | short vulcanization time required (a few seconds) |
Momentive Performance Materials Siloprenâ„¢ FFSL 7031 Fully Fluorinated Liquid Silicone Rubber This LSR elastomer is a fully fluorinated, two-component, platinum (addition/heat) curable, and pumpable silicone elastomer that can be molded and cured with very fast cycle times, at elevated tempe.. |
|||
Mold Temperature | 140 - 230 °C | 284 - 446 °F | short vulcanization time required (a few seconds) |
Momentive Performance Materials Siloprenâ„¢ FFSL 7071 Fully Fluorinated Liquid Silicone Rubber This LSR elastomer is a fully fluorinated, two-component, platinum (addition/heat) curable, and pumpable silicone elastomer that can be molded and cured with very fast cycle times, at elevated tempe.. |
|||
Mold Temperature | 140 - 230 °C | 284 - 446 °F | short vulcanization time required (a few seconds) |
Momentive Performance Materials Siloprenâ„¢ FSL 7641 Fluorinated Liquid Silicone Rubber This LSR elastomer is a fluorinated, two-component, platinum (addition/heat) curable, and pumpable silicone elastomer that can be molded and cured with very fast cycle times, at elevated temperature.. |
|||
Mold Temperature | 140 - 230 °C | 284 - 446 °F | short vulcanization time required (a few seconds) |
Momentive Performance Materials Siloprenâ„¢ FSL 7661 Fluorinated Liquid Silicone Rubber This LSR elastomer is a fluorinated, two-component, platinum (addition/heat) curable, and pumpable silicone elastomer that can be molded and cured with very fast cycle times, at elevated temperature.. |
|||
Mold Temperature | 140 - 230 °C | 284 - 446 °F | short vulcanization time required (a few seconds) |
Momentive Performance Materials Siloprenâ„¢ LIM 6040 Liquid Silicone Rubber - Fast Cure / High Tear This LSR elastomer is a general purpose, two-component, platinum (addition/heat) curable, and pumpable silicone elastomer that can be molded and cured with very fast cycle times, at elevated tempera.. |
|||
Mold Temperature | 140 - 230 °C | 284 - 446 °F | short vulcanization time required (a few seconds) |
Momentive Performance Materials Siloprenâ„¢ LIM 6041 Liquid Silicone Rubber - Healthcare Radio Opaque (X-Ray Detectability) LSR elastomers are a two-component, platinum (addition/heat) curable, and pumpable silicone elastomer that can be molded and cured with very fast cycle times, at elevated temperatures. The molding .. |
|||
Mold Temperature | 140 - 230 °C | 284 - 446 °F | short vulcanization time required (a few seconds) |
Momentive Performance Materials Siloprenâ„¢ LIM 9071E Liquid Silicone Rubber - Self-Bonding This LSR elastomer is a self-bonding, two-component, platinum (addition/heat) curable, and pumpable silicone elastomer that can be molded and cured with very fast cycle times, at elevated temperatur.. |
|||
Mold Temperature | 140 - 230 °C | 284 - 446 °F | short vulcanization time required (a few seconds) |
Momentive Performance Materials Siloprenâ„¢ LSR 2020 Liquid Silicone Rubber - General Purpose This LSR elastomer is a general purpose, two-component, platinum (addition/heat) curable, and pumpable silicone elastomer that can be molded and cured with very fast cycle times, at elevated tempera.. |
|||
Mold Temperature | 140 - 230 °C | 284 - 446 °F | short vulcanization time required (a few seconds) |
Momentive Performance Materials Siloprenâ„¢ LSR 2345/05 Electrically-Conductive Liquid Silicone Rubber This LSR elastomer is an electrically conductive, two-component, platinum (addition/heat) curable, and pumpable silicone elastomer that can be molded and cured with very fast cycle times, at elevate.. |
|||
Mold Temperature | 140 - 230 °C | 284 - 446 °F | short vulcanization time required (a few seconds) |
Momentive Performance Materials Siloprenâ„¢ LSR 2560 Liquid Silicone Rubber - Textile Coating This LSR elastomer is a specialty grade, two-component, platinum (addition/heat) curable, and pumpable silicone elastomer that can be molded and cured with very fast cycle times, at elevated tempera.. |
|||
Mold Temperature | 140 - 230 °C | 284 - 446 °F | short vulcanization time required (a few seconds) |
Momentive Performance Materials Siloprenâ„¢ LSR 2620 Liquid Silicone Rubber - Fast Cure / High Tear This LSR elastomer is a general purpose, two-component, platinum (addition/heat) curable, and pumpable silicone elastomer that can be molded and cured with very fast cycle times, at elevated tempera.. |
|||
Mold Temperature | 140 - 230 °C | 284 - 446 °F | short vulcanization time required (a few seconds) |
Momentive Performance Materials Siloprenâ„¢ LSR 2630 Liquid Silicone Rubber - Fast Cure / High Tear This LSR elastomer is a general purpose, two-component, platinum (addition/heat) curable, and pumpable silicone elastomer that can be molded and cured with very fast cycle times, at elevated tempera.. |
|||
Mold Temperature | 140 - 230 °C | 284 - 446 °F | short vulcanization time required (a few seconds) |
Momentive Performance Materials Siloprenâ„¢ LSR 2640 Liquid Silicone Rubber - Fast Cure / High Tear This LSR elastomer is a general purpose, two-component, platinum (addition/heat) curable, and pumpable silicone elastomer that can be molded and cured with very fast cycle times, at elevated tempera.. |
|||
Mold Temperature | 140 - 230 °C | 284 - 446 °F | short vulcanization time required (a few seconds) |
Momentive Performance Materials Siloprenâ„¢ LSR 2645 Custom Liquid Silicone Rubber - Infant Care This LSR elastomer is a specialty grade, two-component, platinum (addition/heat) curable, and pumpable silicone elastomer that can be molded and cured with very fast cycle times, at elevated tempera.. |
|||
Mold Temperature | 140 - 230 °C | 284 - 446 °F | short vulcanization time required (a few seconds) |
Momentive Performance Materials Siloprenâ„¢ LSR 2651 Liquid Silicone Rubber - Non Post Cure / Low Compression Set This LSR elastomer is a specialty grade, two-component, platinum (addition/heat) curable, and pumpable silicone elastomer that can be molded and cured with very fast cycle times, at elevated tempera.. |
|||
Mold Temperature | 140 - 230 °C | 284 - 446 °F | short vulcanization time required (a few seconds) |
Momentive Performance Materials Siloprenâ„¢ LSR 2660 Liquid Silicone Rubber - Fast Cure / High Tear This LSR elastomer is a general purpose, two-component, platinum (addition/heat) curable, and pumpable silicone elastomer that can be molded and cured with very fast cycle times, at elevated tempera.. |
|||
Mold Temperature | 140 - 230 °C | 284 - 446 °F | short vulcanization time required (a few seconds) |
Momentive Performance Materials Siloprenâ„¢ LSR 2671 Liquid Silicone Rubber - Non Post Cure / Low Compression Set This LSR elastomer is a specialty grade, two-component, platinum (addition/heat) curable, and pumpable silicone elastomer that can be molded and cured with very fast cycle times, at elevated tempera.. |
|||
Mold Temperature | 140 - 230 °C | 284 - 446 °F | short vulcanization time required (a few seconds) |
Momentive Performance Materials Siloprenâ„¢ LSR 2715/50 Liquid Silicone Rubber - Self-Bonding / Self-Lubricating This LSR elastomer is a self-bonding, self-lubricating, two-component, platinum (addition/heat) curable, and pumpable silicone elastomer that can be molded and cured with very fast cycle times, at e.. |
|||
Mold Temperature | 140 - 230 °C | 284 - 446 °F | short vulcanization time required (a few seconds) |
Momentive Performance Materials Siloprenâ„¢ LSR 2740 Liquid Silicone Rubber - Healthcare LSR elastomers are a two-component, platinum (addition/heat) curable, and pumpable silicone elastomer that can be molded and cured with very fast cycle times, at elevated temperatures. The molding .. |
|||
Mold Temperature | 140 - 230 °C | 284 - 446 °F | short vulcanization time required (a few seconds) |
Momentive Performance Materials Siloprenâ„¢ LSR 2740 Liquid Silicone Rubber - Self-Bonding This LSR elastomer is a self-bonding, two-component, platinum (addition/heat) curable, and pumpable silicone elastomer that can be molded and cured with very fast cycle times, at elevated temperatur.. |
|||
Mold Temperature | 140 - 230 °C | 284 - 446 °F | short vulcanization time required (a few seconds) |
Momentive Performance Materials Siloprenâ„¢ LSR 2760 Liquid Silicone Rubber - Self-Bonding This LSR elastomer is a self-bonding, two-component, platinum (addition/heat) curable, and pumpable silicone elastomer that can be molded and cured with very fast cycle times, at elevated temperatur.. |
|||
Mold Temperature | 140 - 230 °C | 284 - 446 °F | short vulcanization time required (a few seconds) |
Momentive Performance Materials Siloprenâ„¢ LSR 3285/50 Liquid Silicone Rubber - Self-Lubricating / Standard This LSR elastomer is a self-lubricating, standard, two-component, platinum (addition/heat) curable, and pumpable silicone elastomer that can be molded and cured with very fast cycle times, at eleva.. |
|||
Mold Temperature | 140 - 230 °C | 284 - 446 °F | short vulcanization time required (a few seconds) |
Momentive Performance Materials Siloprenâ„¢ LSR 3286/50 Liquid Silicone Rubber - Self-Lubricating / Low Compression Set This LSR elastomer is a self-lubricating, low compression set, two-component, platinum (addition/heat) curable, and pumpable silicone elastomer that can be molded and cured with very fast cycle time.. |
|||
Mold Temperature | 140 - 230 °C | 284 - 446 °F | short vulcanization time required (a few seconds) |
Momentive Performance Materials Siloprenâ„¢ LSR 4050 Liquid Silicone Rubber - Healthcare LSR elastomers are a two-component, platinum (addition/heat) curable, and pumpable silicone elastomer that can be molded and cured with very fast cycle times, at elevated temperatures. The molding .. |
|||
Mold Temperature | 140 - 230 °C | 284 - 446 °F | short vulcanization time required (a few seconds) |
Momentive Performance Materials Siloprenâ„¢ LSR 4070 Liquid Silicone Rubber - Healthcare LSR elastomers are a two-component, platinum (addition/heat) curable, and pumpable silicone elastomer that can be molded and cured with very fast cycle times, at elevated temperatures. The molding .. |
|||
Mold Temperature | 140 - 230 °C | 284 - 446 °F | short vulcanization time required (a few seconds) |
Momentive Performance Materials Siloprenâ„¢ LSR 4670 Liquid Silicone Rubber - Healthcare LSR elastomers are a two-component, platinum (addition/heat) curable, and pumpable silicone elastomer that can be molded and cured with very fast cycle times, at elevated temperatures. The molding .. |
|||
Mold Temperature | 140 - 230 °C | 284 - 446 °F | short vulcanization time required (a few seconds) |
Momentive Performance Materials Siloprenâ„¢ LSR TOPCOAT 3719 Liquid Silicone Rubber Specialty Coating Low Surface Friction Coating / USP Class VI Compliancy - Physical Properties are subject to the substrate that is used. |
|||
Mold Temperature | 180 - 230 °C | 356 - 446 °F | |
Lehmann & Voss LUVOCOM® 1104-7452 Polyether ketone, with glass fiber, easy flowing Applications: Automotive industry, mechanical- and precision engineering.Improved strength and stiffnes at elevated temperatures.Improved fatigue properties.Thermic, mechanic and chemical highly str.. |
|||
Mold Temperature | 160 - 230 °C | 320 - 446 °F | |
Lehmann & Voss LUVOCOM® 1114-0717 PAEK, with carbon fiber and PTFE Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Good friction and wear behaviour especially at increased temperatures.Electrically conduct.. |