Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Mold Temperature = 293 °F Product List

Processing Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Processing Properties Metric English Comments
Mold Temperature 145 - 160 °C
293 - 320 °F
Perstorp Compounds 136 Urea-Formaldehyde w/ cellulose filler
A UF-based injection grade designed for hidden parts like sockets, circuit breakers, clamps, switches.Information provided by Perstorp Compounds Inc.
Mold Temperature 145 °C
293 °F
Solvay Specialty Polymers Lavanta® 5115 WH 011 Polyester, High Performance (HPP), 15% Glass Fiber
Lavanta® 5115 WH011 is a 15% glass fiber reinforced, high-performance polyester (HPP) injection molding grade developed specifically for HB LED packaging applications that utilize surface mount ..
Copyright © lookpolymers.com All Rights Reserved