Processing Properties | Metric | English | Comments |
---|---|---|---|
Mold Temperature | 145 - 160 °C | 293 - 320 °F | |
Perstorp Compounds 136 Urea-Formaldehyde w/ cellulose filler A UF-based injection grade designed for hidden parts like sockets, circuit breakers, clamps, switches.Information provided by Perstorp Compounds Inc. |
|||
Mold Temperature | 145 °C | 293 °F | |