Processing Properties | Metric | English | Comments |
---|---|---|---|
Mold Temperature | 46.1 - 60.0 °C | 115 - 140 °F | Cavity mold surface temperature at equilibrium conditions |
NOVA Chemicals Dylark® 510XT Glass Reinforced Engineering Resin Features: Higher toughness product, Excellent stiffness, High heat resistance, Superior adhesion to urethane foamApplications: Instrument panel substrates, Mid-Consoles, Center Stacks, Interior tri.. |
|||
Mold Temperature | 46.1 - 60.0 °C | 115 - 140 °F | Cavity mold surface temperature at equilibrium conditions |
NOVA Chemicals Dylark® 520XT Glass Reinforced Engineering Resin Features: Higher toughness product, Excellent stiffness, High heat resistance, Superior adhesion to urethane foamApplications: Instrument panel substrates, Mid-Consoles, Center Stacks, Interior tri.. |