Polymer Property : Nozzle Temperature = 531 °F Product List

Processing Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Processing Properties Metric English Comments
Nozzle Temperature 277 - 310 °C
531 - 590 °F
Average value: 294 °C Grade Count:3
Overview of materials for Polystyrene + Polyphenylene Ether, Unreinforced
This property data is a summary of similar materials in the MatWeb database for the category "Polystyrene + Polyphenylene Ether, Unreinforced". Each property range of values reported is minimum and ..
Nozzle Temperature 277 - 335 °C
531 - 635 °F
Average value: 312 °C Grade Count:7
Overview of materials for Polystyrene + Polyphenylene Ether, Glass + Mineral Filler
This property data is a summary of similar materials in the MatWeb database for the category "Polystyrene + Polyphenylene Ether, Glass + Mineral Filler". Each property range of values reported is mi..
Nozzle Temperature 277 - 285 °C
531 - 545 °F
Elastocon TPE Technologies Elastocon® STK55PA Thermoplastic Elastomer
Elastocon® STK55PA thermoplastic elastomer has been developed for applications that require soft rubber-like properties and a good surface finish. Elastocon® STK55PA is well suited for consumer go..
Nozzle Temperature 277 - 285 °C
531 - 545 °F
Elastocon TPE Technologies Elastocon® STK56PA Thermoplastic Elastomer
Elastocon® STK56PA thermoplastic elastomer has been developed for applications that require soft rubber-like properties and a good surface finish. Elastocon® STK56PA is well suited for consumer go..
Nozzle Temperature 277 - 316 °C
531 - 601 °F
Average value: 297 °C Grade Count:3
Overview of materials for Polystyrene + Polyphenylene Ether, Glass Filler
This property data is a summary of similar materials in the MatWeb database for the category "Polystyrene + Polyphenylene Ether, Glass Filler". Each property range of values reported is minimum and ..