Processing Properties | Metric | English | Comments |
---|---|---|---|
Nozzle Temperature | 218 °C | 424 °F | Die |
DuPont 20 Series 2010 Specialty Polyethylene Resin DuPont 2010 specialty low density polyethylene resin is characterized by low melt index and intermediate crystallinity. This product, produced via a unique polymerization process, has outstanding fl.. |
|||
Nozzle Temperature | 218 °C | 424 °F | Die |
DuPont 20 Series 20-6064 Specialty Polyethylene Resin DuPont 20-6064 specialty low density polyethylene resin is characterized by low melt index and intermediate crystallinity. This product, produced via a unique polymerization process, has outstanding.. |
|||
Nozzle Temperature | 218 °C | 424 °F | Die |
DuPont 20 Series DPE 20 Specialty Polyethylene Resin DuPont 20 specialty low density polyethylene resin is characterized by low melt index and intermediate crystallinity. This product, produced via a unique polymerization process, has outstanding flex.. |
|||
Nozzle Temperature | 218 °C | 424 °F | |
Lubrizol Estane® 58144 Thermoplastic Polyurethane Type: Estane® 58144 is a 65D Polyether-type thermoplastic polyurethane (TPU) compound.Features: FDA (contact Lubrizol for details). Pre-drying: 2 hours at 104C (220F) in Dehumidifying Hopper Dryer.. |