Material Notes:
DuPont 2010 specialty low density polyethylene resin is characterized by low melt index and intermediate crystallinity. This product, produced via a unique polymerization process, has outstanding flexibility and environmental stress crack resistance and contains a mold release agent. Typical Applications: Injection blow molded closures where close thread tolerances are required; Pharmaceutical and medical bottles and closures; Personal care containers and closures; Low pressure air and water tubing. Features & Benefits: Superior resistance to environmental stress cracking; High flexibility; Good heat stability; Excellent color; Odor free; Excellent chemical resistance; Good mold release performance; Nontoxic.Information provided by DuPont Packaging Polymers.
Physical Properties Metric English Comments
Density 0.920 g/cc
0.0332 lb/in³
ASTM D792
Melt Flow 1.9 g/10 min

@Load 2.16 kg,
Temperature 190 °C
1.9 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Shore D 48
48
ASTM D2240
Tensile Strength, Ultimate 14.7 MPa
2130 psi
ASTM D638
Tensile Strength, Yield 9.60 MPa
1390 psi
ASTM D638
Elongation at Break 560 %
560 %
ASTM D638
Modulus of Elasticity 0.186 GPa
27.0 ksi
ASTM D638
Flexural Modulus 0.183 GPa
26.5 ksi
ASTM D790
Izod Impact, Notched NB
NB
ASTM D256
0.430 J/cm

@Temperature -40.0 °C
0.806 ft-lb/in

@Temperature -40.0 °F
ASTM D256
Thermal Properties Metric English Comments
Melting Point 95.0 °C
203 °F
Freezing Point via DSC/ASTM D3418
109 °C
228 °F
Upon Melting via DSC/ASTM D3418
Deflection Temperature at 0.46 MPa (66 psi) 44.0 °C
111 °F
ASTM D648
Vicat Softening Point 95.0 °C
203 °F
ASTM D1525
Brittleness Temperature <= -76.0 °C
<= -105 °F
ASTM D746
Optical Properties Metric English Comments
Refractive Index 1.51
1.51
ASTM D542
Processing Properties Metric English Comments
Processing Temperature 218 °C
424 °F
Typical Nozzle Ext. and Manifold temp for injection blow molding.
Nozzle Temperature 218 °C
424 °F
Die