Processing Properties Metric English Comments
Nozzle Temperature 299 - 327 °C
570 - 620 °F
Ravago Manufacturing Americas Hylex® P1007L Polycarbonate
Information provided by Ravago
Nozzle Temperature 299 - 327 °C
570 - 620 °F
Ravago Manufacturing Americas Hylex® P1307L Polycarbonate
Entec's proprietary products include a full range of compounds in the Nylon 6/6, Nylon 6, ABS, PBT, Polycarbonate, PC/ABS, PC/ASA, PC/PBT, and PPO/PPE resin families.Information provided by Ente..
Nozzle Temperature 299 - 327 °C
570 - 621 °F
Styron CALIBREâ„¢ 2061-6 Polycarbonate Resin
Overview: CALIBREâ„¢ 2061-6 resin is suitable for steam and ethylene oxide sterilization required by the health care industry. CALIBRE 2061-6 provides excellent heat resistance, impact strength, ..