Processing Properties | Metric | English | Comments |
---|---|---|---|
Nozzle Temperature | 95.0 - 115 °C | 203 - 239 °F | Barrel Nozzle Temp |
Perstorp Compounds 136 Urea-Formaldehyde w/ cellulose filler A UF-based injection grade designed for hidden parts like sockets, circuit breakers, clamps, switches.Information provided by Perstorp Compounds Inc. |