Processing Properties Metric English Comments
Nozzle Temperature 95.0 - 115 °C
203 - 239 °F
Barrel Nozzle Temp
Perstorp Compounds 136 Urea-Formaldehyde w/ cellulose filler
A UF-based injection grade designed for hidden parts like sockets, circuit breakers, clamps, switches.Information provided by Perstorp Compounds Inc.