Processing Properties | Metric | English | Comments |
---|---|---|---|
Nozzle Temperature | 174 - 185 °C | 345 - 365 °F | |
Ravago Manufacturing Americas Hylac® FR134 ABS Entec's proprietary products include a full range of compounds in the Nylon 6/6, Nylon 6, ABS, PBT, Polycarbonate, PC/ABS, PC/ASA, PC/PBT, and PPO/PPE resin families.Information provided by Rava.. |