Processing Properties | Metric | English | Comments |
---|---|---|---|
Injection Velocity | 40.0 - 65.0 mm/sec | 1.57 - 2.56 in/sec | Average value: 47.7 mm/sec Grade Count:13 |
Overview of materials for Acrylonitrile Butadiene Styrene (ABS)/Nylon Blend This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS)/Nylon Blend". Each property range of values reported is minimum an.. |