Polymer Property : Injection Velocity = 0.984 in/sec Product List

Processing Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Processing Properties Metric English Comments
Injection Velocity 10.0 - 25.0 mm/sec
0.394 - 0.984 in/sec
Molding a 6 gram (shot weight) gasket with a 50 ton injection molding machine; screw diameter of 25 mm
Premix Thermoplastics PRETHERM TPE 1050 Thermoplastic Elastomer, Boron Nitride / SEBS compound
PRETHERM TPE 1050 is a thermoplastic elastomer based highly thermally conductive compound intended primarily for heat dissipation. It is used as gap filler between processor and heat sink or co-mold..
Injection Velocity 10.0 - 25.0 mm/sec
0.394 - 0.984 in/sec
Molding a 6 gram (shot weight) gasket with a 50 ton injection molding machine; screw diameter of 25 mm
Premix Thermoplastics PRETHERM TPE 1050 Thermoplastic Elastomer, Boron Nitride / SEBS compound
PRETHERM TPE 1050 is a thermoplastic elastomer based highly thermally conductive compound intended primarily for heat dissipation. It is used as gap filler between processor and heat sink or co-mold..
Injection Velocity 10.0 - 25.0 mm/sec
0.394 - 0.984 in/sec
Molding a 6 gram (shot weight) gasket with a 50 ton injection molding machine; screw diameter of 25 mm
Premix Thermoplastics PRETHERM TPE 1075 Thermoplastic Elastomer, Boron Nitride / SEBS compound
PRETHERM TPE 1075 is a thermoplastic elastomer based highly thermally conductive compound intended primarily for heat dissipation. It can be used as gap filler between processor and heat sink or co-..
Injection Velocity 13.0 - 25.0 mm/sec
0.512 - 0.984 in/sec
Zhejiang Double Fish YS-G030 30% Long Fiber Glass Reinforced Polypropylene
Features high strength, good surface quality, and easy processing. Typical applications include automobile (bumper back beam, arm rest core, instrument panel, mudflap), machinery, electronics, comm..
Injection Velocity 13.0 - 25.0 mm/sec
0.512 - 0.984 in/sec
Zhejiang Double Fish YS-G040 40% Long Fiber Glass Reinforced Polypropylene
Features high strength, good surface quality, and easy processing. Typical applications include automobile (bumper back beam, arm rest core, instrument panel, mudflap), machinery, electronics, comm..
Injection Velocity 13.0 - 25.0 mm/sec
0.512 - 0.984 in/sec
Zhejiang Double Fish YS-G050 50% Long Fiber Glass Reinforced Polypropylene
Features high strength, good surface quality, and easy processing. Typical applications include automobile (bumper back beam, arm rest core, instrument panel, mudflap), machinery, electronics, comm..