Polymer Property : Front Barrel Temperature = 435 °F Product List

Processing Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Processing Properties Metric English Comments
Front Barrel Temperature 193 - 224 °C
379 - 435 °F
PolyOne Versalloy™ HC 9220-70 Thermoplastic Elastomer (TPE)
Versalloy™ HC 9220-70 is a TPV alloy targeted for extrusion and injection molding healthcare applications such as medical tubing, disposable medical items and soft-touch overmolding for surgical gr..
Front Barrel Temperature 193 - 224 °C
379 - 435 °F
PolyOne Versalloy™ HC 9220-80 Thermoplastic Elastomer (TPE)
Versalloy™ HC 9220-80 is a TPV alloy targeted for extrusion and injection molding healthcare applications such as medical tubing, disposable medical items and soft-touch overmolding for surgical gr..
Front Barrel Temperature 210 - 224 °C
410 - 435 °F
Ravago Manufacturing Americas Hylac® GP74G20 ABS, 20% Glass Fiber Reinforced
Entec's proprietary products include a full range of compounds in the Nylon 6/6, Nylon 6, ABS, PBT, Polycarbonate, PC/ABS, PC/ASA, PC/PBT, and PPO/PPE resin families.Information provided by Rava..
Front Barrel Temperature 210 - 224 °C
410 - 435 °F
Ravago Manufacturing Americas Hylac® GP74G30 ABS, 30% Glass Fiber Reinforced
Entec's proprietary products include a full range of compounds in the Nylon 6/6, Nylon 6, ABS, PBT, Polycarbonate, PC/ABS, PC/ASA, PC/PBT, and PPO/PPE resin families.Information provided by Rava..
Front Barrel Temperature 191 - 224 °C
376 - 435 °F
Ineos Nova Zylar® 221 Clear Impact Modified Acrylic Copolymer  (discontinued **)
Features: High clarityEnhanced mold releaseGood elongationStyrenic processing advantagesExcellent property retention after ETO and gamma sterilization Applications: DisplaysMedical devicesOffice acc..
Front Barrel Temperature 191 - 224 °C
376 - 435 °F
Ineos Nova Zylar® 390 Clear Impact Modified Acrylic Copolymer  (discontinued **)
Features: Excellent clarityHigh flexural modulusGood toughness and elongationStyrenic processing advantagesExcellent property retention after ETO and gamma sterilizationMeets USP XXIII specification..
Front Barrel Temperature 191 - 224 °C
376 - 435 °F
Ineos Nova Zylar® 533 Clear Impact Modified UV Stabilized Acrylic Copolymer  (discontinued **)
Features: High clarityStyrenic processing advantagesExcellent property retention after ETO and gamma sterilizationExcellent indoor light stabilityHigh elongation and ductilityApplications: Appliance..
Front Barrel Temperature 191 - 224 °C
376 - 435 °F
Ineos Nova Zylar® 220 Clear Impact Modified Acrylic Copolymer  (discontinued **)
Features:High clarity Good elongation Styrenic processing advantages Excellent property retention after gamma and ETO sterilization Meets USP XXIII specifications for Class VI plasticsApplications:D..
Front Barrel Temperature 191 - 224 °C
376 - 435 °F
Ineos Nova Zylar® 330 Clear Impact Modified Acrylic Copolymer  (discontinued **)
Features:Clarity and stiffness Good heat distortion resistance Styrenic processing advantages Excellent property retention after gamma and ETO sterilization Meets USP XXIII specifications for Class ..
Front Barrel Temperature 191 - 224 °C
376 - 435 °F
Ineos Nova Zylar® 530 Clear Impact Modified Acrylic Copolymer  (discontinued **)
Features:High clarityStyrenic processing advantagesExcellent property retention after ETO and gamma sterilizationMeets USP XXIII specifications for Class VI plasticsUL94 HB @ 1.5 mm for uncolored ma..
Front Barrel Temperature 191 - 224 °C
376 - 435 °F
Ineos Nova Zylar® 535 Clear Impact Modified Acrylic Copolymer  (discontinued **)
Features: High clarity, strength and toughnessStyrenic processing advantagesExcellent property retention after ETO and gamma sterilizationAnti-stat packageEnhanced mold releaseUL 94HB @ 1.5 mm for a..
Front Barrel Temperature 191 - 224 °C
376 - 435 °F
Ineos Nova Zylar® 631 Clear Impact Modified Acrylic Copolymer  (discontinued **)
Features:Outstanding practical toughness and ductilityStyrenic processing advantagesExcellent property retention after ETO and gamma sterilizationUSP Class VI compliantCustom colors and enhancement ..
Front Barrel Temperature 210 - 224 °C
410 - 435 °F
Ravago Manufacturing Americas Hylac® GP30G ABS, 30% Glass Fiber Reinforced
Entec's proprietary products include a full range of compounds in the Nylon 6/6, Nylon 6, ABS, PBT, Polycarbonate, PC/ABS, PC/ASA, PC/PBT, and PPO/PPE resin families.Information provided by Rava..
Front Barrel Temperature 191 - 224 °C
376 - 435 °F
Ineos Nova Zylar® 94-580-A High Performance Styrenic, Acrylic Copolymer  (discontinued **)
Excellent heat distortion temperature, High clarity, strength and toughness, Enhanced mold releaseApplications: Industrial covers and housings, Paper towel dispenser covers, Appliance partsInjection..