Middle Barrel Temperature 80.0 - 120 °C
176 - 248 °F
Trelleborg Horda Cable E6352-A2 Bonded Semiconductive Shielding And Conductor Screen
E6352-A2 is a crosslinkable semiconductive compound based on ethylene copolymer compound, designed for conductor screen and insulation shield applications in XLPE and EPDM insulated cables with bond..