Processing Properties | Metric | English | Comments |
---|---|---|---|
Middle Barrel Temperature | 329 - 354 °C | 625 - 670 °F | |
Oxford Polymers Polysulfone PSF P170-64170 White PSU Product Description: Polysulfone injection molding grade, precolored white Processing and Delivery Form: Pellets and Injection Molding Special Characteristics: Continuous use up to 300(f)Informatio.. |
|||
Middle Barrel Temperature | 329 °C | 625 °F | |
MTI ThermoStran® PPA-40C Long Carbon Fiber Compound ThermoStran® is custom designed long fiber thermoplastic compound (LFC) engineered to meet specific end use requirements. Continuous fibers are pultruded to yield pellets with fibers equivalent t.. |
|||
Middle Barrel Temperature | 329 °C | 625 °F | |
MTI ThermoStran® PPA-50G Long Glass Fiber Compound ThermoStran® is custom designed long fiber thermoplastic compound (LFC) engineered to meet specific end use requirements. Continuous fibers are pultruded to yield pellets with fibers equivalent t.. |