Processing Properties | Metric | English | Comments |
---|---|---|---|
Sintering Temperature | 1580 °C @Time 3600 sec |
2880 °F @Time 1.00 hour |
|
Nabaltec GRANALOX® NM 9212 B Ceramic Body, Binder Free Nabaltec offers ceramic bodies with different alumina content as free-of-binder grades. With the addition of necessary amount of water (approx. 20 %) these grades can be directly used for slip casti.. |
|||
Sintering Temperature | 1580 °C | 2880 °F | |
Nabaltec GRANALOX® NM 9212 E Ceramic Bodies Nabaltec`s GRANALOX® Ceramic bodies are produced under rigid quality control of green and sintered density, shrinkage, porosity, loss on ignition and granulate size. The properties of the corundum .. |
|||
Sintering Temperature | 1580 °C | 2880 °F | |
Nabaltec GRANALOX® NM 9212 F Ceramic Bodies Nabaltec`s GRANALOX® Ceramic bodies are produced under rigid quality control of green and sintered density, shrinkage, porosity, loss on ignition and granulate size. The properties of the corundum .. |
|||
Sintering Temperature | 1580 - 1700 °C | 2880 - 3090 °F | Interval (dense ceramic parts) |
Nabaltec GRANALOX® NM 9620 Ceramic Bodies Nabaltec`s GRANALOX® Ceramic bodies are produced under rigid quality control of green and sintered density, shrinkage, porosity, loss on ignition and granulate size. The properties of the corundum .. |
|||
Sintering Temperature | 1580 - 1700 °C | 2880 - 3090 °F | Interval (dense ceramic parts) |
Nabaltec GRANALOX® NM 9620 F Ceramic Bodies Nabaltec`s GRANALOX® Ceramic bodies are produced under rigid quality control of green and sintered density, shrinkage, porosity, loss on ignition and granulate size. The properties of the corundum .. |
|||
Sintering Temperature | 1580 - 1680 °C | 2880 - 3060 °F | Interval (dense ceramic parts) |
Nabaltec GRANALOX® NM 9634 F Ceramic Body Nabaltec's GRANALOX® Ceramic bodies are produced under rigid quality control of green and sintered density, shrinkage, porosity, loss on ignition and granulate size. The properties of the corundum .. |