Fill Speed 300 - 600 mm/sec
11.8 - 23.6 in/sec
Peripheral Screw Speed
Solvay Technyl® A 246M Nylon 66, Impact Grade, EH0
Unreinforced and modified polyamide 66, with improved impact resistance, heat stabilized, for injection molding.Technyl A 246m offers an excellent notched impact resistance at low temperatures makin..
Fill Speed 300 - 600 mm/sec
11.8 - 23.6 in/sec
Peripheral Screw Speed
Solvay Technyl® A 246M Nylon 66, Impact Grade, EH50
Unreinforced and modified polyamide 66, with improved impact resistance, heat stabilized, for injection molding.Technyl A 246m offers an excellent notched impact resistance at low temperatures makin..
Fill Speed 300 - 600 mm/sec
11.8 - 23.6 in/sec
Peripheral Screw Speed
Solvay Technyl® A218 Heat Stabilized Nylon 66
Information provided by Rhodia; Rhodia has been acquired by Solvay.
Fill Speed 300 - 600 mm/sec
11.8 - 23.6 in/sec
Peripheral Screw Speed
Solvay Technyl® A238 Unfilled, Heat Stabilized, Impact Modified Nylon 66
Information provided by Rhodia; Rhodia has been acquired by Solvay.
Fill Speed 200 - 600 mm/sec
7.87 - 23.6 in/sec
Peripheral Screw Speed
Solvay Technyl® C 218 MT25 V15 25% Mineral, 15% Glass Filled, Heat Stabilized Nylon 6
Information provided by Rhodia; Rhodia has been acquired by Solvay.
Fill Speed 200 - 600 mm/sec
7.87 - 23.6 in/sec
Peripheral Screw Speed
Solvay Technyl® C 218 V50 50% Glass Filled, Heat Stabilized Nylon 6
Information provided by Rhodia; Rhodia has been acquired by Solvay.
Fill Speed 300 - 600 mm/sec
11.8 - 23.6 in/sec
Peripheral Screw Speed
Solvay Technyl® C206F Unfilled, Fast Cycle Nylon 6
Information provided by Rhodia; Rhodia has been acquired by Solvay.
Fill Speed 200 - 600 mm/sec
7.87 - 23.6 in/sec
Peripheral Screw Speed
Solvay Technyl® C216V15 15% Glass Filled Nylon 6
Information provided by Rhodia; Rhodia has been acquired by Solvay.
Fill Speed 200 - 600 mm/sec
7.87 - 23.6 in/sec
Peripheral Screw Speed
Solvay Technyl® C216V25 25% Glass Filled Nylon 6
Information provided by Rhodia; Rhodia has been acquired by Solvay.
Fill Speed 200 - 600 mm/sec
7.87 - 23.6 in/sec
Peripheral Screw Speed
Solvay Technyl® C216V30 30% Glass Filled Nylon 6
Information provided by Rhodia; Rhodia has been acquired by Solvay.
Fill Speed 200 - 600 mm/sec
7.87 - 23.6 in/sec
Peripheral Screw Speed
Solvay Technyl® C218V30 30% Glass Filled, Heat Stabilized Nylon 6
Information provided by Rhodia; Rhodia has been acquired by Solvay.