Processing Properties Metric English Comments
Cure Time 5.000000 min

@Temperature 150 °C
0.08333334 hour

@Temperature 302 °F
ACC QGel 301 QSI Quantum Silicones High Strength Gel
QGel 301 is a clear, very soft, tough, moderately cross-linked, silicone polymer. Silicone gels are used to provide protection from vibration, thermal or mechanical shock. Silicone gels also provide..
Cure Time 5.000000 min

@Temperature 150 °C
0.08333334 hour

@Temperature 302 °F
ACC QGel 311 QSI Quantum Silicones General Purpose Silicone Gel
QGel 311 is a clear, fast cure, tough moderately cross-linked silicone polymer. Silicone gels are used to provide protection from vibration and thermal or mechanical shock. Silicone gels also provid..