Processing Properties | Metric | English | Comments |
---|---|---|---|
Cure Time | 5.000000 min @Temperature 150 °C |
0.08333334 hour @Temperature 302 °F |
|
ACC QGel 301 QSI Quantum Silicones High Strength Gel QGel 301 is a clear, very soft, tough, moderately cross-linked, silicone polymer. Silicone gels are used to provide protection from vibration, thermal or mechanical shock. Silicone gels also provide.. |
|||
Cure Time | 5.000000 min @Temperature 150 °C |
0.08333334 hour @Temperature 302 °F |
|
ACC QGel 311 QSI Quantum Silicones General Purpose Silicone Gel QGel 311 is a clear, fast cure, tough moderately cross-linked silicone polymer. Silicone gels are used to provide protection from vibration and thermal or mechanical shock. Silicone gels also provid.. |