Processing Properties | Metric | English | Comments |
---|---|---|---|
Cure Time | 10080 - 30240 min @Temperature 20.0 °C |
168.0 - 504.0 hour @Temperature 68.0 °F |
(1-3 weeks) |
Abatron AboCast/AboCure 8006-11 Epoxy AboCast/AboCure 8006-11 is a clear dielectric casting, adhesive, and encapsulating compound. It is a 2-component, radiation-resistant, low-viscosity plasticized epoxy system. It is virtually unaffec.. |