Processing Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Processing Properties Metric English Comments
Cure Time 720 - 1200 min

@Temperature 25.0 °C
12.0 - 20.0 hour

@Temperature 77.0 °F
Resin Technology Group TIGA 202-EX High Performance, Fast Cure Adhesive
Mix ratio 2 to 1 by volume.TIGA 202-EX is a two-part epoxy adhesive offering outstanding shear tensile and peel adhesion. TIGA 202-EX offers a 20 minute pot life and good hardness development within..
Cure Time 960 - 1200 min

@Temperature 70.0 °C
16.0 - 20.0 hour

@Temperature 158 °F
1st step
Abatron AboCast 8502-7/AboCure 8502-7 Colorless, Low-Exotherm Epoxy Casting Compound
AboCast 8502-7/AboCure 8502-7 is a rigid, heat cured, colorless, low-exotherm epoxy casting compound for larger masses. It is a 2-component structural and dielectric liquid system with extremely low..